Tips for successful welding

Please always observe the most important rules for successful welding when working with a PUK precision welder :

Grinding electrodes

Always work with a well-ground electrode!
This is the only way to achieve optimum results.
The Lampert electrode grinding motor is best suited for this purpose:
To grind the electrode tips, the electrodes should be held at an angle of 15° to the rotating diamond wheel and rotated between the fingers.
There are guide holes with diameters of 0.6, 0.8, 1.0 and 1.3 mm.

Contact workpiece - welding machine

Good electrical conductivity is very important in welding technology.
This means that, firstly, the connections must be as flat as possible and, secondly, the contacting tool mustbe made of a material with the highest possible electrical conductivity.

Perfect electrical contact between the workpiece and the contact terminal must always be ensured, i.e. the workpiece must be connected to the terminal of the connecting cable at a metallically bright point or via a contacting tool.

Welding with low pressure

Do not exert any pressure on the electrode, just hold the workpiece against the tip.
This light touch must be maintained until welding is complete.

Stable position

Never weld “freehand”, i.e. always place both hands on a support (work table).

Restoration work, for example, can take several hours.
Large workpieces in particular also require a good range of movement.
In exceptional cases, the handpiece can therefore also be guided directly by hand.

Power and pulse duration

If in doubt, please start with rather low values for power and pulse duration and increase your energy settings step by step.
Increasing the pulse duration generally has a greater effect on the energy emitted than increasing the power.
For materials with increased thermal conductivity, such as copper, several welding points close together can be helpful to bring the material up to temperature.

Electrode tip

It is also important how far the electrode tip protrudes from the handpiece nozzle.
The shorter the electrode is clamped, the better the protection provided by the argon.
In general, the electrode should not protrude more than 4 to 5 mm from the nozzle.

The angle at which the workpiece touches the electrode tip significantly influences the flow direction of the welding spot, as the material tends to follow the arc

For welding tasks in low-lying or hard-to-reach areas, the electrode can be clamped so that it protrudes slightly longer from the nozzle.
In this case, the gas flow can be slightly increased.

Set the flow rate and electrodes correctly

Always weld with the gas flow rate of approx. 2 l/min recommended by us.
The electrode should not protrude longer than necessary from the handpiece nozzle, ideally approx. 4 – 6 mm or adjusted with the gauge in the handpiece holder arm of a Lampert welding microscope.